| Properties |
Value |
CC60S001A |
CC60S002A |
CC60S002B |
| Thermal Properties |
|
|
|
|
| Max. Service Temperature |
(oC) |
1600 |
1600 |
1600 |
| Permanent Linear Change |
% |
-0.20 |
+/-1.5 |
+/-1.5 |
| After heating at Temp. |
oC |
|
1500 |
1500 |
| Thermal Conductivity at 600 oC |
kcal/hr.m.oC |
1.07 |
|
|
| Thermal Conductivity at1000 oC |
kcal/hr.m.oC |
1.20 |
|
|
| Chemical Properties |
|
|
|
|
| Alumina (Al2O3) |
% |
60.0 |
60.0 |
60.0 |
| Iron Oxide (Fe2O3) |
% |
1.4 |
1.5 |
1.5 |
| Physical Properties |
|
|
|
|
| Cold Crushing Strength at 110oC |
kg/cm2 |
400 |
350 |
400 |
| Dry Density |
g/cm3 |
2.23 |
2.20 |
2.30 |
| Max. Grain Size of Aggregates |
mm |
5.0 |
6.0 |
6.0 |
| Approx. Amount of Water Required for Casting |
% |
10 |
|
|