15% SIC BASED BRICKS |
| Properties | Value | SB15S002A (13-17%) |
| Thermal Properties | ||
| Permanent Linear Change | % | +/-0.6 |
| After heating at Temp. | oC | 1200 |
| Thermal Conductivity at 600 oC | kcal/hr.m.oC | 2.45 |
| Chemical Properties | ||
| Alumina (Al2O3) | % | 46.0 |
| Iron Oxide (Fe2O3) | % | 1.2 |
| Silicon Carbide (SiC) | % | 13-17 |
| Physical Properties | ||
| Cold Crushing Strength at 110oC | kg/cm2 | 500 |
| Dry Density | g/cm3 | 2.50 |